Mechanical and tribological behaviour of nano scaled
3.1. Effect of silicon carbide on composite microstructure and morphology The methodology used to introduce silicon carbide platelets into the aluminium frame-work permitted the addition of a maximum of 2.5 wt.%-silicon carbide. The delivered materials display uniform microstructure (Figure 6), and they demonstrate uniform dis-